美国杜邦POM 900P NC010物性表①原料描述部分规格级别高流动 其它 注塑外观颜色该料用途较多模穴与较不易填充的薄肉成型品。备注说明加工特性:高流动性低黏度表面经润滑树脂,DELRIN 900P有优异的成型特性。 产品:与DELRIN 500相近,但稍微低的拉伸延伸率和冲击强度。POM美国杜邦900P详细说明原料技术数据性能项目试验条件[状态]测试方法测试数据数据单位物理性能比重ASTM D-7921.42模收缩2.2-2.4%吸水量50%相对湿度ASTM D-5700.22%吸水量浸渍平衡点ASTM D-5700.90%吸水量24小时浸渍ASTM D-5700.25%机械性能洛氏硬度MASTM D-78594挠曲系数23℃ASTM D-7903220MPa挠曲系数100℃ASTM D-7901030MPa洛氏硬度RASTM D-785120破裂点拉伸变形量23℃ASTM D-63825%IZOD冲击强度23℃ASTM D-25671j/m抗拉伸冲击强度长试片23℃ASTM D-1822250kj/m2挠曲系数70℃ASTM D-7901720MPaIZOD冲击强度缺口-40℃ASTM D-25655j/m拉伸强度70℃ASTM D-63848MPa挠曲疲劳忍耐限度50%RH,23℃,106周期ASTM D-67132MPa破裂点拉伸变形量-55℃ASTM D-63810%压缩应力23℃,10%变形ASTM D-695121MPa破裂点拉伸变形量70℃ASTM D-638180%破裂点拉伸变形量100℃ASTM D-638>260%挠曲系数-55℃ASTM D-7904730MPa拉伸强度23℃ASTM D-63869MPa弹性系数23℃ASTM D-6383640MPa抗剪强度23℃ASTM D-73266MPa挠曲系数122℃ASTM D-790755MPa破裂点拉伸变形量122℃ASTM D-638>260%挠曲变形强度23℃ASTM D-79097MPa拉伸强度122℃ASTM D-63826MPaIZOD冲击强度无缺口23℃ASTM D-2561620j/m拉伸强度100℃ASTM D-63836MPa负载变形量140kg/cm2,50℃ASTM D-6210.5%压缩应力23℃,1%变形ASTM D-69535MPa拉伸强度-55℃ASTM D-638101MPa电气性能介电强度瞬间Short time(2.3mm)ASTM D-14919.7kv/mm容积电阻率23℃,0.2%含水量ASTM D-2571×1015Ω.cm抗电弧3.1mmASTM D-495220sec介电常数50%RH,23℃,102~106HzASTM D-1503.7Ω.cm介电因数50%RH,23℃,106HzASTM D-1500.005热性能线性热膨胀系数29~60℃ASTM D-69612.210-5m/m℃自燃性UL 94HB热传导系数0.37W/mk线性热膨胀系数60~104℃ASTM D-69613.710-5m/m℃线性热膨胀系数104~160℃ASTM D-69614.910-5m/m℃热畸变温度1.8MPaASTM D-648136℃热畸变温度0.5MPaASTM D-648172℃线性热膨胀系数-40~29℃ASTM D-69610.410-5m/m℃熔点℃ASTM D-2133175高抗冲再生料塑料生产工艺流程大部分是来自于电器产品(如电视机后盖)、玩具、文教用品、装饰材料等等。 1.首先把色别分开,因为ABS和IPS不是专业人员的话很难分别,一定要仔细挑开,因改苯和ABS不能合拢,如果合拢产品则报废,如文教用品玩具镀铬喷漆较多一定挑开。 2.处理:退镀、退漆,因化学处理一定配比,另外要用防护用品和容器,否则可能损伤身体。 3.清洗条件:放一点皂粉和去油剂,再用清水洗清,要注意废水的环境污染。 4.把洗净料:A.晒干;B.烘干;C.甩干机甩干。等这些材料晒干后再配颜色放一些副料。 5.专用挤出机上车挤出,水冷切粒,然后包装标号出厂。