| 性能项目 | 试验条件 | 测试方法 | 测试数据 | |
| 比重 | ASTMD792 | 1.63 | g/cm3 | |
| 收缩率-流动(3.00mm) | ASTMD955 | 0.300.90 | % | |
| 吸水率(24hr) | ASTMD570 | 0.050 | % | |
| 洛氏硬度(M级) | ASTMD785 | 95 | ||
| 抗张强度(屈服) | ASTMD638 | 155 | MPa | |
| 伸长率(断裂) | ASTMD638 | 1.9 | % | |
| 弯曲模量 | ASTMD790 | 12000 | MPa | |
| 弯曲强度(屈服) | ASTMD790 | 220 | MPa | |
| 悬壁梁缺口冲击强度 | ASTMD256 | 90 | J/m | |
| 载荷下热变形温度 | 0.45MPa,未退火 | ASTMD648 | 245 | °C |
| 载荷下热变形温度 | 1.8MPa,未退火 | ASTMD648 | 235 | °C |
| 熔融温度 | DSC | 255 | °C | |
| 线形热膨胀系数-流动 | ASTMD696 | 2.5E-5 | cm/cm/°C | |
| RTIElec | UL746 | 130 | °C | |
| RTIImp | UL746 | 130 | °C | |
| RTI | UL746 | 130 | °C | |
| 体积电阻率 | ASTMD257 | 1.0E 18 | ohmscm | |
| 介电强度(2.00mm) | ASTMD149 | 25 | kV/mm | |
| 耐电弧性 | ASTMD495 | 130 | sec | |
| UL阻燃等级 | UL94 | HB | ||